I have now obtained a sample of polycaprolactone granules and used it in place of Polymorph. It works perfectly to make rods for the RepRap extruder. I used granules of CAPA 6800 polycaprolactone (2-Oxepanone, homopolymer; molecular weight 80,000, CAS number: 24980-41-4) from
Solvay Interox Ltd.
Baronet Works
Lower Walton
Warrington WA4 6HB
U.K.
+44 (0) 1925 643210
The Solvay website is here. CAPA 6800 is supplied by the company in 20 kg paper sacks, or 500 kg bags.
There is a more complete write-up on polymorph on the RepRap Wiki.
I've contacted the NZ distributor and I'm attempting to arrange samples and bulk product at this end.
ReplyDeleteVik :v)
Okay Adrian, reading your twiki on CAPA 6800 I understand that this is the material you want to unify work on for this iteration of the project. If that's not so I need to know.
ReplyDeleteI talked to Solvay's US agent in Houston just now and he is sending me a 5 kg sample. That should last me a while if I'm careful.
Jeff Neidinger in Houston gave me a price range of $5.30-3.50/lb for CAPA 6800. That means that a single, 20 kg sack will cost something like $234. That's a bit steep compared to something like polypropylene, but not outrageous.
This looks like a really good material. :-)
I think that polycaprolactone, polymorph and friendly plastic are all essentially the same thing, despite slight differences in the FTIR shown on the wiki. We sincerely hope that 25 kg would run a RepRap machine for quite a while, including making several other machines...
ReplyDeleteShould be.
ReplyDeleteThis comment has been removed by a blog administrator.
ReplyDeleteThis comment has been removed by a blog administrator.
ReplyDeleteMy own experience in working with polyethylene suggests that you will lose some of your polymer to oxidation. Much of that oxidation might be curbed with more careful heating processes than I had, though.
ReplyDeleteAs well, I expect that painting conducting strips onto parts will present some problems in segregating polymer and conducting material in the recycling process.
The bugbear is little particles of non-plastic crud in the recycled stuff clogging the nozzle of your extruder. It's bad enough keeping 'em out with new plastic granules.
ReplyDeleteMind you, if we're using a large deposition nozzle for bulk filling or moulding, we can tolerate more impurities.
I've reused Polymorph a lot and it goes "Old Underwear" grey but retains plasticity. One batch went yellow. Not underwear - Polymorph.
Vik :v)
I've observed HDPE going yellow on the surface when it was overheated. I took the colouring to be oxidation.
ReplyDelete